黄志华, 李暑宏, 苏秀珠. 低品位金矿粉矿制粒—堆浸试验研究[J]. 矿产综合利用, 2014, 35(1).
    引用本文: 黄志华, 李暑宏, 苏秀珠. 低品位金矿粉矿制粒—堆浸试验研究[J]. 矿产综合利用, 2014, 35(1).
    Huang Zhihua, Li Shuhong, Su Xiuzhu. Experimental Research on Granulation-heap Leaching for a Low-grade Gold Ore[J]. Multipurpose Utilization of Mineral Resources, 2014, 35(1).
    Citation: Huang Zhihua, Li Shuhong, Su Xiuzhu. Experimental Research on Granulation-heap Leaching for a Low-grade Gold Ore[J]. Multipurpose Utilization of Mineral Resources, 2014, 35(1).

    低品位金矿粉矿制粒—堆浸试验研究

    Experimental Research on Granulation-heap Leaching for a Low-grade Gold Ore

    • 摘要: 对某低品位金矿粉矿进行制粒-堆浸试验,考察了固化剂、固化剂用量、水耗、固化时间等对粉矿制粒的影响,并对制粒矿进行堆浸试验,探索制粒矿的浸出性能。试验得到粉矿制粒的最佳条件:水泥用量7kg/t,水耗为30L/t,成球粒径 2.36mm-20mm,固化水分为10%,固化时间大于24小时。粉矿经制粒后渗透性大大提高,柱浸试验尾渣金品位低于0.07g/t,堆浸试验尾渣金品位低于0.089g/t,浸出效果良好。为低品位金矿粉矿的处理提供了指导意义。

       

      Abstract: Researches on granulation-heap leaching of low-grade gold fine ores were carried out in this paper, granulation factors such as bonder, consumption, water dosage, and curing time were investigated, and heap-leaching tests were taken to identify leaching performance of pellet ores. Results indicated that the best conditions of granulation are as follow: consumption of cement is 7kg/t, water dosage is 30L/t, pellet size between 2.36mm and 20mm, curing time above 24h. Permeability of pellet ores improved greatly, leaching tailings of column leaching and heap leaching are 0.06g/t, 0.089g/t, respectively.

       

    /