某铜铁矿选矿实验

    Test on Mineral Processing Technology for the Copper-iron Ore

    • 摘要: 针对某铜铁矿矿石性质特点,采用先浮-后磁工艺流程,配合使用选择性好的捕收剂酯-112,实现了矿石的综合回收。采用“先浮-后磁”工艺,即将原矿磨至-74 μm 70% ,铜回路采用一次粗选、三次精选产出铜精矿;铜扫选尾矿经过一次磁选产出铁精矿。闭路实验获得铜精矿中铜的品位为20.72%,铜回收率为80.76%;铜精矿中金品位43.91 g/t,回收率86.29%,铁精矿品位为66.38%,铁回收率为94.20%,铁精矿中有害元素硫含量仅为0.16%。

       

      Abstract: Aiming at the characteristics of a copper-iron ore, we adopt the process of first flotation and then magnetic process, together with the use of ester-112, which is a good selective collector, to realize the comprehensive recovery of the ore. Using the “first flotation - then magnetic” process, the original ore is ground to -74 μm 70%, copper circuit using one roughing, three cleaning for the output of copper concentrate.copper sweeping tailings after a magnetic separation output of iron ore concentrate. Closed-circuit tests obtained copper grade of 20.72% and recovery rate of 80.76% in the copper concentrate, gold grade of 43.91 g/t and recovery rate of 86.29% in the copper concentrate, iron grade of 66.38% recovery rate of 94.20% in the iron concentrate, among which the content of the harmful elements of the sulfur is only 0.16%.

       

    /

    返回文章
    返回