新疆某高方解石型萤石矿浮选实验

    Flotation of a High-calcium Fluorite Ore in Xinjiang

    • 摘要: 新疆某高方解石型萤石矿,萤石含量25.47%,方解石含量41.67%,为有效抑制方解石,获得合格的萤石精矿,提高矿物回收率,开展浮选实验研究工作。在磨矿细度-0.074 mm ±65%的条件下,使用捕收剂EM-OL8,抑制剂EMN,调整剂SSB,采用“两次粗选一次扫选八次精选,中矿Ⅱ-Ⅷ顺序返回,中矿Ⅰ与扫选精矿返回粗选Ⅱ”闭路实验流程,获得了产率22.02%,品位97.38%,回收率84.20%的萤石精矿,为后续工业生产提供了技术依据。

       

      Abstract: A high-calcite type fluorite ore in Xinjiang contains 25.47% fluorite and 41.67% calcite. To effectively inhibit calcite, thereby obtaining a qualified fluorite concentrate and improving the mineral recovery rate, researchers carried out a flotation test research. At the condition of a grinding fineness of -0.074 mm 65%, the test used collector EM-OL8, depressant EMN, and modifier SSB, and the researchers adopted a closed-circuit test process of "two roughing one scavenging eight cleaning , with middlings Ⅱ-Ⅷ returning in sequence, and middling Ⅰ and scavenging concentrate returning to roughing Ⅱ". The test obtained fluorite concentrate was achieved with a yield of 22.02%, a CaF2 grade of 97.38%, and a recovery rate of 84.20%, which provides a technical foundation for subsequent industrial production.

       

    /

    返回文章
    返回